Nikkellegeringen Hânlieding elektrode ENi-1 weld fabrication makings
GEMISCHE KOMPONET:
ALLOY (wt%) | C | Mn | Si | Ni | Fe | Ti | Cu | P | S |
GB / T REGELS | 0.10 | 0,75 | 1.20 | ≥92 | 0,70 | 1,0-4,0 | 0.20 | 0.02 | 0.015 |
AWS REGELS | 0.10 | 0,75 | 1.25 | ≥92 | 0,75 | 1,0-4,0 | 0.25 | 0.03 | 0.02 |
EXEMPEL WAARDE | 0.046 | 0.06 | 0.82 | 95,5 | 0.12 | 2.7 | 0.01 | 0.007 | 0.001 |
MEGANISCHE EIENDOM:
BESIT | YIELD STRENGT (MPa) | EXTENSION STRENGTH (MPa) | IMAPACT WAARDE J/℃ | ELONGATION(%) | ||||
GB / T REGELS | 200 | 410 | - | 18 | ||||
AWS REGELS | - | 410 | - | 20 | ||||
EXEMPEL WAARDE | 310 | 435 | - | 29 |
Oanrikkemandearre weldingparameters:
DIAMETER SPESIFIKASJES (mm) | 2,6*300 | 3,2*350 | 4,0*350 | |||||||
ELEKTRISITEIT (Amp) | H/W | 65-95 | 70-115 | 95-145 |
Titanium-calcium hân elektrodes, nominale gearstalling (persint troch gewicht) is 95Ni-2.5Ti.
Stabile bôge, prachtige foarmjen, lytse plons, maklike slagferwidering, goede porositeitresistinsje.
De fusearre metaal hat goede meganyske eigenskippen, waarmte ferset, corrosie ferset, fúzje en crack ferset.
Cr-Mo stielen rige welding materialen en elektrode surfacing welding materialen wurde in soad brûkt yn petroleum raffinaazjetechnyk
-
158.000 ton Suez tanker
Supercore SG
GEMISCHE KOMPONET:
ALLOY (wt%) | C | Mn | Si | Ni | Fe | Ti | Cu | P | S |
GB / T REGELS | 0.10 | 0,75 | 1.20 | ≥92 | 0,70 | 1,0-4,0 | 0.20 | 0.02 | 0.015 |
AWS REGELS | 0.10 | 0,75 | 1.25 | ≥92 | 0,75 | 1,0-4,0 | 0.25 | 0.03 | 0.02 |
EXEMPEL WAARDE | 0.046 | 0.06 | 0.82 | 95,5 | 0.12 | 2.7 | 0.01 | 0.007 | 0.001 |
MEGANISCHE EIENDOM:
BESIT | YIELD STRENGT (MPa) | EXTENSION STRENGTH (MPa) | IMAPACT WAARDE J/℃ | ELONGATION(%) | ||||
GB / T REGELS | 200 | 410 | - | 18 | ||||
AWS REGELS | - | 410 | - | 20 | ||||
EXEMPEL WAARDE | 310 | 435 | - | 29 |
Oanrikkemandearre weldingparameters:
DIAMETER SPESIFIKASJES (mm) | 2,6*300 | 3,2*350 | 4,0*350 | |||||||
ELEKTRISITEIT (Amp) | H/W | 65-95 | 70-115 | 95-145 |