Nikkel alloys TIG ERNiCrFe-7A Soldering jointing
GEMISCHE KOMPONET:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S |
GB / T REGELS | - | - | - | - | - | - | - | - | - | - |
AWS REGELS | 0.04 | 1.00 | 0,50 | 28.0-31.5 | Rem | 0,50 | 7.0-11.0 | 0,5-1,0 | 0.02 | 0.015 |
EXEMPEL WAARDE | 0.028 | 0.15 | 0.11 | 29.8 | 59.03 | 0.06 | 9.8 | 0.86 | 0.001 | 0.002 |
MEGANISCHE EIENDOM:
BESIT | YIELD STRENGT (MPa) | EXTENSION STRENGTH (MPa) | IMAPACT WAARDE J/℃ | ELONGATION(%) | Heat behanneling | ||||||
GB / T REGELS | - | - | - | - | - | ||||||
AWS REGELS | - | - | - | - | - | ||||||
EXEMPEL WAARDE | - | 760 | 133 / Keamertemperatuer | 37 | 607°C*25h |
Nikkel-chroom-izer nikkel-base alloy gas welding tried, nominale gearstalling is 60% Ni-29% Cr-9% Fe-0,75% Nb.
Goede meganyske eigenskippen fan smelte metaal, benammen wjerstân tsjin lege plastic kraken (DDC).
Hege Cr ynhâld makket it hawwe poerbêst stress corrosie kraken ferset yn suver wetter omjouwing ûnder strieling betingst. Stabile bôge, prachtige foarming, goede trochstreaming fan smelte izer, mei poerbêste weldingprosesprestaasjes.
GEMISCHE KOMPONET:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S |
GB / T REGELS | - | - | - | - | - | - | - | - | - | - |
AWS REGELS | 0.04 | 1.00 | 0,50 | 28.0-31.5 | Rem | 0,50 | 7.0-11.0 | 0,5-1,0 | 0.02 | 0.015 |
EXEMPEL WAARDE | 0.028 | 0.15 | 0.11 | 29.8 | 59.03 | 0.06 | 9.8 | 0.86 | 0.001 | 0.002 |
MEGANISCHE EIENDOM:
BESIT | YIELD STRENGT (MPa) | EXTENSION STRENGTH (MPa) | IMAPACT WAARDE J/℃ | ELONGATION(%) | Heat behanneling | ||||||
GB / T REGELS | - | - | - | - | - | ||||||
AWS REGELS | - | - | - | - | - | ||||||
EXEMPEL WAARDE | - | 760 | 133 / Keamertemperatuer | 37 | 607°C*25h |